How to get the best results from FusionLock Nano Adhesive and FusionLock Build Surface Cleaner.
1. Start with a clean build plate
- Shake the Build Surface Cleaner well.
- Spray the whole build surface.
- Wait 1 to 3 minutes for it to soak.
- Wipe with a microfiber cloth under warm running water until the plate is visibly clean, then dry it.
Handle the plate by its edges afterwards. Skin oils and dust get between the plate and the first layer and weaken adhesion.
2. Apply the adhesive
Apply a thin, even coat over the area you will print on, using the dauber tip, the wide brush or the spray, and let it dry before you print.
3. Print
Print with your usual settings for the filament. One coat lasts many prints, up to 100 or more depending on part size and material.
4. Remove the part
Let the build plate cool before removing parts. If you pull a part off while it is still hot, especially with high-temperature filaments, some adhesive can come away on the bottom of the print. It is water-soluble and rinses off with warm water.
5. Know when to re-coat
When the film on the plate begins to flake, heat has used it up. Wash the plate with Build Surface Cleaner and warm water, then apply a fresh coat.
Compatible filaments
- Standard: PLA, PLA+, ABS, PETG, TPU
- High performance: nylon, carbon and glass fiber filled, ASA, PVA, HIPS, polycarbonate (PC), PEI, PEEK, PEKK
- Not for: polypropylene (PP). For PP, cover the plate with packaging tape instead.
Build surfaces
Smooth and textured PEI, stock Creality plates, glass and borosilicate glass, Garolite (G-10), spring steel, FR4.
Common questions
My print still warps. What should I check?
Make sure the plate was cleaned before coating, that the bed is at the temperature your filament maker recommends, and that the first layer is pressed into the plate and not laid on top of it. Drafts and a cold room make warping worse, particularly with ABS, ASA and nylon.
There is adhesive on the bottom of my print.
The part was probably removed while the plate was still hot. Rinse it under warm water.
Do I need ventilation?
Use a fume extractor or good ventilation when printing filaments that give off high levels of VOCs.
Still stuck?
Contact us and tell us your printer, build plate and filament.